| Tensile Strength, Ultimate | 55 | MPa | EN ISO 527-1:2012 | X |
| Elongation at Break | 31.6 | % | EN ISO 527-1:2012 | X |
| Youngs Module | 1680 | MPa | EN ISO 527-1:2012 | X |
| Bending Strength | 54.2 | MPa | EN ISO 178:2019 | X |
| Bending Modulus | 1290 | MPa | EN ISO 178:2019 | X |
| Charpy Unnotched | 179 | kJ/m² | EN ISO 179-1:2010 | X |
| Hardness | 76 | Shore D | EN ISO 868:2005 | — |